金属热处理 ›› 2026, Vol. 51 ›› Issue (2): 16-22.DOI: 10.13251/j.issn.0254-6051.2026.02.003

• 组织与性能 • 上一篇    下一篇

复合制造TC25G钛合金构件的组织与力学性能

王洋1,2,3,4, 韩佳兴1,2, 罗威豪1,2, 程序2,3,5, 刘栋2,5   

  1. 1.北京航空航天大学 材料科学与工程学院, 北京 100191;
    2.北京航空航天大学 大型金属构件增材制造国家工程实验室, 北京 100191;
    3.北京航空航天大学 宁波创新研究院, 浙江 宁波 315800;
    4.中国航空技术国际控股有限公司, 北京 100027;
    5.北京航空航天大学 前沿科学技术创新研究院, 北京 100191
  • 收稿日期:2025-09-17 修回日期:2025-12-11 发布日期:2026-03-05
  • 通讯作者: 刘 栋,副研究员,博士,E-mail:09294@buaa.edu.cn
  • 作者简介:王 洋(1988—),男,正高级工程师,硕士,主要研究方向为钛合金增材制造,E-mail:wangy709@163.com。
  • 基金资助:
    国家科技重大专项(2019-Ⅶ-0003-0143);国家自然科学基金(52090044)

Microstructure and mechanical properties of hybrid manufactured TC25G titanium alloy component

Wang Yang1,2,3,4, Han Jiaxing1,2, Luo Weihao1,2, Cheng Xu2,3,5, Liu Dong2,5   

  1. 1. School of Materials Science and Engineering, Beihang University, Beijing 100191, China;
    2. National Engineering Laboratory for Additive Manufacturing of Large Metal Components, Beihang University, Beijing 100191, China;
    3. Ningbo Institute of Innovation, Beihang University, Ningbo Zhejiang 315800, China;
    4. AVIC International Holding Corporation, Beijing 100027, China;
    5. Frontier Science and Technology Innovation Research Institute, Beihang University, Beijing 100191, China
  • Received:2025-09-17 Revised:2025-12-11 Published:2026-03-05

摘要: 采用激光定向能量沉积+锻造相结合的复合制造技术制备了TC25G钛合金件,并对其进行固溶时效处理,对比研究了沉积态及热处理态TC25G钛合金件的组织和力学性能。结果表明,激光定向能量沉积+锻造复合制造TC25G钛合金件的界面冶金结合良好,无明显缺陷,从热影响区过渡到锻造区,初生α相含量逐渐增加。经固溶时效处理后,锻造基体区与热影响区组织差异性降低,复合制造试样的室温和高温抗拉强度分别提高14.7%和23.3%,断后伸长率分别提高118.2%和318.0%。复合制造TC25G钛合金件的拉伸断裂位置位于锻造基体区,表明结合区并没有成为“弱区”。

关键词: 复合制造, 激光定向能量沉积, 锻造, 组织, 拉伸性能, 硬度

Abstract: TC25G titanium-alloy components were produced by a hybrid manufacture route that coupled laser-directed energy deposition (LDED) with forging, followed by a solution + aging heat treatment. Microstructure and mechanical properties were systematically compared between the as-deposited and heat-treated conditions. The results show that LDED/forging interface exhibits sound metallurgical bonding free of lack-of-fusion or solidification cracks. Moving from the heat-affected zone (HAZ) into the forged substrate, the volume fraction of primary α phase increases progressively. After solution treatment and aging, the difference in microstructure between the forged substrate and the heat-affected zone is reduced, the tensile strength at room temperature and high temperature of the hybrid manufactured specimen increases by 14.7% and 23.3%, respectively, and the elongation after fracture increases by 118.2% and 318.0%, respectively. The tensile fracture positions of the TC25G titanium alloy components are all located in the forged substrate, indicating that the bonding area is not a "weak zone".

Key words: hybrid manufacture, laser-directed energy deposition, forging, microstructure, tensile properties, hardness