[1] 陈亦兵. 链条销轴用40Cr钢表面感应有效硬化层深度、硬度与剪切强度关系的研究[J]. 机械传动, 2021, 45(10): 170-175. Chen Yibing. Study on the relationship between the depth, hardness and shear strength of the inductively effective hardening case on the surface of 40Cr steel pin for chain[J]. Journal of Mechanical Transmission, 2021, 45(10): 170-175. [2] 毕 廉, 刘冬杰, 薛 峰. 钢脚裂纹原因分析[J]. 金属热处理, 2024, 49(6): 305-307. Bi Lian, Liu Dongjie, Xue Feng. Cause analysis of steel foot cracks[J]. Heat Treatment of Metals, 2024, 49(6): 305-307. [3] 张丽伟, 刘素芬, 王 凡, 等. 50CrVA钢板簧淬火开裂原因分析[J]. 金属热处理, 2015, 40(12): 201-203. Zhang Liwei, Liu Sufen, Wang Fan, et al. Analysis on quenching cracks of 50CrVA steel leaf spring[J]. Heat Treatment of Metals, 2015, 40(12): 201-203. [4] 姜如松, 廖永红. 40CrMnMo钢单体泵泵体淬火开裂分析及对策[J]. 金属热处理, 2016, 41(12): 187-191. Jiang Rusong, Liao Yonghong. Quenching crack analysis and counter measures of 40CrMnMo steel single pump body[J]. Heat Treatment of Metals, 2016, 41(12): 187-191. [5] 蒋庆彬, 张左治, 朱正伟, 等. 42CrMoA钢销轴调质开裂失效分析及改进措施[J]. 金属热处理, 2020, 45(9): 244-247. Jiang Qingbin, Zhang Zuozhi, Zhu Zhengwei, et al. Failure analysis and improvement measures of quenched and tempered crack on 42CrMoA steel pin shaft[J]. Heat Treatment of Metals, 2020, 45(9): 244-247. [6] 陈巧菊. 40Cr钢齿轮坯料淬裂原因浅析[J]. 广西师范学院学报(自然科学版), 2011(S1): 8-9. [7] 刘 玉, 左训伟, 陈乃录, 等. 淬火纵向裂纹的有限元模拟[J]. 材料热处理学报, 2019, 40(3): 160-167. Liu Yu, Zuo Xunwei, Chen Nailu, et al. Finite element simulation of longitudinal quenching crack[J]. Transactions of Materials and Heat Treatment, 2019, 40(3): 160-167. [8] 孔学云, 马认琦, 于海永, 等. 40CrMnMo钢轴心管淬火开裂原因分析及预防措施[J]. 金属热处理, 2010, 35(2): 91-93. Kong Xueyun, Ma Renqi, Yu Haiyong, et al. Analysis on quenching crack of 40CrMnMo steel center tube and its countermeasures[J]. Heat Treatment of Metals, 2010, 35(2): 91-93. |