Heat Treatment of Metals ›› 2020, Vol. 45 ›› Issue (7): 86-89.DOI: 10.13251/j.issn.0254-6051.2020.07.018

• PROCESS RESEARCH • Previous Articles     Next Articles

Optimization of heat treatment process of 980 MPa cold-rolling dual phase steel

Chen Zhuo1, Jin Bin2, Wang Chengsi2, Liu Jingbao1, Kuang Shuang1, Liu Liping1, Wang Zhao1, Li Mengxing1, Yang Mingwei1, Wang Jinrong1   

  1. 1. Technology Center, HBIS Group Tangsteel Company, Tangshan Hebei 063016, China;
    2. Tangshan Iron & Steel Group Will Automation Co., Ltd., Tangshan Hebei 063016, China
  • Received:2019-12-20 Online:2020-07-25 Published:2020-09-07

Abstract: Effects of soaking temperature, slow cooling temperature and overaging temperature during continuous annealing on mechanical properties and microstructure of DP980 steel were investigated by means of Gleeble-3500 annealing simulator, optical microscope and tensile testing machine. The results indicate that the martensite content of the DP980 steel is increased with the increase of soaking temperature, which leads to the enhancement of yield strength and tensile strength accordingly. The optimal soaking temperature is 780 ℃. Effect of slow cooling temperature on mechanical properties of DP980 steel is investigated based on the control capability of equipment, and 670 ℃ is selected as the optimal temperature. Besides, the overaging temperature has been possessed large adjustment range on yield strength of DP980 steel, which can reduce the yield ratio significantly. With the increase of overaging temperature, the martensite content is remained stable and a little carbide is precipitated, which reduces the martensite strength and improves the plasticity of DP980 steel. The optimal parameters of soaking temperature, slow cooling temperature and overaging temperature are 780, 670, 320 ℃, respectively.

Key words: DP980 steel, continuous annealing, microstructure, mechanical properties